不同晶型碳酸钙表面改性及CaCO3/PDMS超疏水涂层制备
DOI:
CSTR:
作者:
作者单位:

1.湖北大学材料科学与工程学院;2.陕西科技大学轻工科学与工程学院;3.湖北大学

作者简介:

通讯作者:

中图分类号:

TB742

基金项目:

广西创新驱动发展专项(2018AA21013);湖北大学青年科学基金(201911304000001)


Surface modification of calcium carbonate with different crystal forms and preparation of CaCO3/PDMS superhydrophobic coating
Author:
Affiliation:

1.School of Materials Science and Engineering, Hubei University;2.School of Materials Science and Engineering,Hubei University;3.College of bioresources chemical and materials engineering, Shaanxi University of Science and Technology;4.Key Laboratory of Green Preparation and Application for Functional Materials,Ministry of Education,School of Materials Science and Engineering,Hubei Engineering Research Center for Green Industrialization Technology of Industrial Waste,Hubei University

Fund Project:

Innovation-driven Development Project of Guangxi, China(2018AA21013); Youth Science Foundation of Hubei University(201911304000001)

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    摘要:超疏水涂层是一种表面具有特殊浸润性的涂膜,因其在自清洁、油水分离、抗菌、防腐蚀等领域的优异表现,得到广泛关注和研究。该文利用硬脂酸钠(NaSt)和油酸钠(NaOL)对文石型和方解石型两种CaCO3粉体进行表面改性,然后利用改性的CaCO3粉体与聚二甲基硅氧烷(PDMS)共混,喷涂得到CaCO3/PDMS基超疏水涂层。结果表明,当NaSt和NaOL用量(以反应溶液总质量计)为5%时,CaCO3粉体改性效果最好,所制备的CaCO3/PDMS涂层疏水性最佳。同时考察了不同晶型CaCO3用量对涂层疏水性能的影响,结果发现,当CaCO3和PDMS质量比为1.5:1时,CaCO3/PDMS涂层接触角>150°,具有超疏水性。对其自清洁能力及稳定性测试结果表明,玻璃板涂层表面的亚甲基蓝污染物可以完全随着液滴冲走,没有残留,且在经过500 mL 5 m/s的水流冲击下,接触角仍达140°以上,展现了涂层工作时效的持久性和稳定性。

    Abstract:

    Abstract: Superhydrophobic coating is a kind of coating with special wettability on the surface. it has received extensive attention and research because of its excellent performance in the fields of self-cleaning, oil-water separation, antibacterial, anti-corrosion, etc. In this paper, sodium stearate (NaSt) and sodium oleate (NaOL) were used to modify the surface of aragonite and calcite CaCO3 powders, and then the modified CaCO3 powders were blended with polydimethylsiloxane (PDMS) to obtain CaCO3/PDMS based superhydrophobic coatings. The results showed that when the content of NaSt and NaOL was 5% of the substance participating in the reaction, the modification effect of CaCO3 powder was the best, and the hydrophobicity of the prepared CaCO3/PDMS coating was the best. At the same time, the influence of the amount of CaCO3 with different crystal forms on the hydrophobicity of the coating was investigated. The results showed that when the mass ratio of CaCO3 to PDMS was 1.5:1, the contact angle of the CaCO3/PDMS coating was>150°, and the coating was super hydrophobic. The test results of its self-cleaning ability and stability showed that the methylene blue pollutants on the surface of the glass plate coating could be completely washed away with the liquid droplets without residue, and the contact angle was still more than 140°under the impact of 500 mL water with a speed of 5 m/s, which showed the durability and stability of the coating working age.

    参考文献
    相似文献
    引证文献
引用本文

罗帅帅,古卫乐,操未青,刘雷鹏,胡攀,田键.不同晶型碳酸钙表面改性及CaCO3/PDMS超疏水涂层制备[J].精细化工,2023,40(8):

复制
分享
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2022-10-21
  • 最后修改日期:2023-02-01
  • 录用日期:2023-02-02
  • 在线发布日期: 2023-08-17
  • 出版日期:
文章二维码