Degradation pattern and hydrolysis mechanism of polyester particles temporary plugging agent
Author:
Affiliation:

College of Chemical and Environmental Engineering,Yangtze University

Fund Project:

Joint Fund for Enterprise Innovation and Development of National Natural Science Foundation of China (Grant Nos. U19B6003-05)

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    以聚乳酸(PLA)、聚乙交酯(PGA)、聚己二酸-对苯二甲酸丁二醇酯(PBAT)三种典型的聚酯类颗粒为代表,探究聚酯类颗粒作为暂堵剂的降解规律和水解机理,并对其封堵性能进行评价。结果表明,盐酸和氢氧化钠质量浓度越大,温度越高,完全降解时间越短,且同一质量浓度下,氢氧化钠溶液中降解更快,90℃下,100 g/L氢氧化钠溶液中,PLA、PGA、PBAT的完全降解时间分别为15h、12h、18d。借助FTIR、XRD、SEM阐明了聚酯类颗粒暂堵剂的水解机理:降解初期,酯基开始水解,颗粒表面出现孔洞,颗粒体积略微减小;随着降解的进行,水解优先发生在无定形区,结晶度增大,羰基指数减小,羟基指数增大,颗粒表面孔洞增多,体积进一步缩小;降解后期,结晶区开始水解,结晶度减小,聚合物分子链大量断裂,直至完全降解。封堵实验表明,注入聚酯类颗粒暂堵剂的质量浓度越大,封堵层越致密,承压能力越强,且承压能力由大到小依次为PLA、PGA、PBAT。

    Abstract:

    Three typical polyester-based particles, polylactic acid (PLA), polyglycolide (PGA) and polybutylene adipate-terephthalate (PBAT), were used as representatives to investigate the degradation law and hydrolysis mechanism of polyester-based particles as temporary plugging agents and evaluate their blocking performance. The results showed that the larger the mass concentration of hydrochloric acid and sodium hydroxide, the higher the temperature, the shorter the complete degradation time, and at the same mass concentration, the degradation in sodium hydroxide solution was faster, and the complete degradation time of PLA, PGA and PBAT in 100 g/L sodium hydroxide solution at 90 ℃ was 15h, 12h and 18d, respectively. The hydrolysis mechanism of polyester particle plugging agent was elucidated with the help of FTIR, XRD and SEM: at the early stage of degradation, the ester group began to hydrolyze, holes appeared on the surface of the particles, and the volume of the particles was slightly reduced; as the degradation proceeded, the hydrolysis preferentially took place in the amorphous zone, the crystallinity increased, the carbonyl index decreased, the hydroxyl index increased, and the holes on the surface of the particles increased and the volume was further reduced; at the late stage of degradation, the hydrolysis of crystalline zone started, the crystallinity decreased, and a large number of polymer molecular chains were broken until the complete degradation. The blocking experiment shows that the larger the mass concentration of the injected polyester particles plugging agent is, the denser the blocking layer is, the stronger the pressure-bearing capacity is, and the pressure-bearing capacity is PLA, PGA, PBAT in descending order.

    参考文献
    相似文献
    引证文献
引用本文

胡安邦,于小荣,彭凯南,杨周,杨欢,苏高申.聚酯类颗粒暂堵剂的降解规律及水解机理[J].精细化工,2024,41(9):

复制
分享
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2023-09-07
  • 最后修改日期:2023-12-19
  • 录用日期:2023-12-04
  • 在线发布日期: 2024-09-10
  • 出版日期:
文章二维码