聚酯型聚氨酯弹性体的制备及性能
DOI:
CSTR:
作者:
作者单位:

沈阳工业大学 石油化工学院

作者简介:

通讯作者:

中图分类号:

TQ334.1

基金项目:


Preparation and performance of PUE based on GCHD-modified PBCHA as soft segment
Author:
Affiliation:

School of Petrochemical Technology,Shenyang University of Technology

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    摘要:以戊二酸环氧环己烷二酯二醇(GCHD)改性聚己二酸丁二醇酯(modified polybutylene adipate 缩写PBCHA)为软段(soft segment 缩写SS),二环己基甲烷二异氰酸酯(HMDI)为硬段(hard segment 缩写HS)合成了聚酯型聚氨酯弹性体(PUE)。通过FTIR、TG、DSC、拉伸性能测试、断裂伸长率测试等手段研究了HMDI、GCHD、催化剂添加量对PUE的热稳定性、力学性能等的性能影响。结果表明,随着HMDI质量分数、GCHD摩尔分数的增加,拉伸强度呈现先增大后减小的趋势,其中HMDI质量分数为21%,GCHD摩尔分数4%,拉伸强度达到最大为16.44 Mpa,断裂伸长率减小。断裂伸长率随着改性剂含量的增多而降低,最佳的断裂伸长率为2337.38%。HMDI质量分数对T10%、T50%、Tmax热分解温度影响最大,GCHD摩尔分数次之,催化剂质量分数最小,随着HMDI质量分数增多T10%、T50%、Tmax逐渐增大,最高的T10%热分解温度可达362.65 ℃,T50%热分解温度372.69,Tmax为405.95 ℃。

    Abstract:

    Abstract: Polyester polyurethane elastomers (PUEs) were synthesized using glutarate epoxycyclohexane diglycol (GCHD), modified polybutylene adipate (PBCHA) as the soft segment (SS), and dicyclohexylmethane diisocyanate (HMDI) as the hard segment (HS). The effects of HMDI, glutarate GCHD, and catalyst addition on the thermal stability and mechanical properties of PUE were studied by FTIR, TG, DSC, tensile performance test, elongation at break test, etc. The results show that with the increase of HMDI mass fraction and GCHD molar fraction, the tensile strength first increases and then decreases, in which the mass fraction of HMDI is 21%, the molar fraction of GCHD is 4%, the tensile strength reaches the maximum of 16.44 Mpa, and the elongation at break decreases. The elongation at break decreased with the increase of modifier content, and the optimal elongation at break was 2337.38%.The elongation at break decreased with the increase of modifier content, and the optimal elongation at break was 2337.38%. With the increase of HMDI mass fraction, the highest thermal decomposition temperature of T10%, T50% and Tmax reached 362.65 °C, the highest T50% thermal decomposition temperature was 372.69 °C, and Tmax was 405.95 °C.

    参考文献
    相似文献
    引证文献
引用本文

曲淼,李继新.聚酯型聚氨酯弹性体的制备及性能[J].精细化工,2025,42(3):

复制
分享
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2024-10-25
  • 最后修改日期:2024-11-08
  • 录用日期:2024-11-20
  • 在线发布日期: 2025-03-14
  • 出版日期:
文章二维码