    With the raw material maleic anhydride, mixed alcohols and styrene, the copolymer maleic anhydride mixed alcohols ester- styrene(PMST) is synthetized, the reaction conditions are investigated and the pour point depressant effect is tested. The suitable esterifications are, molar ratio of mixed alcohols and material maleic anhydride is 2:1, esterification time is 3h, amount of catalyst is 1.5%, amount of esterification solvent is 20%; and the suitable polymerizations are, molar ratio of styrene and maleic anhydride mixed alcohols is 1:1, amount of polymerization solvent is 50%, polymerization temperature is 80℃, amount of initiator is 1.5%, polymerization time is 3h. IR and 1H-NMR spectra confirm the structure of products. When the addition dose of PMST is 0.4%(based on the mass of wax oil), and the heat treatment temperature is 70℃, PMST can make the pour point of wax oil used in experiment decline 26℃,this pour point point can make high freezing point wax oil have an ideal fluidity in room temperature even lower temperature.

    Reference
    Related
    Cited by
Get Citation
Related Videos

Share
Article Metrics
  • Abstract:
  • PDF:
  • HTML:
  • Cited by:
History
  • Received:February 06,2013
  • Revised:April 04,2013
  • Adopted:April 08,2013
  • Online: June 28,2013
  • Published:
Article QR Code